Fri Jan 18, 2008 6:58 am

I am nearing the completion of a Brutus10 system, and fired it up for the first time last night. I noticed that the pilot light sure puts out a lot of soot. I am using converted kegs.
Also- does anyone have any experience repassivating stainless kegs that have started to show rust? I have hydrofluoric acid and was wondering if that could be used in place of nitric acid. :idea: :?:
Terrazza
 
Posts: 48
Joined: Tue Dec 27, 2005 5:48 pm

Fri Jan 18, 2008 7:12 am

John Palmer is a metalurgist by trade, and his website www.howtobrew.com has a whole section on passivating SS.
User avatar
bergerandfries
 
Posts: 175
Joined: Fri Nov 17, 2006 1:45 pm

Fri Jan 18, 2008 12:41 pm

Adjust your air intake on that pilot light... you should not get soot.
BUB
Lunch Meet "Limpian" Gold Medalist (x2) 2006
Winner of <b>NO PANTS</b> award 2006 and 2007
Make your own beer website... starting at $10 per YEAR.
www.bubweb.com & www.momenttoponder.com
User avatar
bub
Global Moderator
 
Posts: 3396
Joined: Sat Dec 31, 2005 2:06 pm
Location: Greater Nashvegas

Fri Jan 18, 2008 5:44 pm

You also want to make sure that the flame isn't impinging (touching anything), if it does it will soot. Depending on the type you have you may have to adjust the metal housing it has or adjust it if its touching your burner.

Barry
User avatar
Eagle Creek Brewer
 
Posts: 209
Joined: Fri Feb 09, 2007 5:59 pm

Sun Jan 20, 2008 8:32 am

Cool. Bub, I just turned down that pilot light and no soot. Since I had som hydroflouric acid solution, I poured a little inside where the rust was, and it dissolved instantly away. I also had some really fine sand paper that I wetted in the acid and lightly went over where the rust was. Rinsed it well with distilled water and dried right away. I'll see if this works or not. I'm not planning on touching those kegs for a good week. Has anyone else ever had issues with rust? :?:
Terrazza
 
Posts: 48
Joined: Tue Dec 27, 2005 5:48 pm

Sun Jan 20, 2008 9:07 am

I'm no metalurgist, but if I recall correctly, you need a nitric acid based solvent to properly passivate SS.

That doesn't mean that the hydroflouric won't work, I'm just trying to regurgitate something I think I remember hearing Rock Candy say. Point is to help you validate what you did is right.

HTH-
-B'Dawg
BJCP GM3 Judge & Mead
"Lunch Meat. It's an acquired taste....." -- Mylo
User avatar
BDawg
 
Posts: 4993
Joined: Tue Jul 31, 2007 5:27 pm
Location: North Bend, WA

Sun Jan 20, 2008 9:19 am

Since you have HF I presume you understand it's extremely dangerous, just thought I'd point it out for others. HF is an excellent rust remover used with nitric to clean stainless, nitric is used to passivate.
User avatar
BrewTa2
Global Moderator
 
Posts: 3454
Joined: Sat Jan 12, 2008 8:46 am
Location: Hannibal, MO

Sun Jan 20, 2008 11:21 am

BrewTa2 wrote:Since you have HF I presume you understand it's extremely dangerous, just thought I'd point it out for others. HF is an excellent rust remover used with nitric to clean stainless, nitric is used to passivate.


I was just going to post that. I used HF when I worked in a materials lab. That shit was in the hood 100% of the time. It is very nasty stuff.
Image<see, it's getting better.
User avatar
Test_Engineer
 
Posts: 273
Joined: Sun Oct 07, 2007 4:33 pm
Location: A2/Ypsi, MI

Next

Return to Brewing Sculptures

Who is online

Users browsing this forum: No registered users

A BIT ABOUT US

The Brewing Network is a multimedia resource for brewers and beer lovers. Since 2005, we have been the leader in craft beer entertainment and information with live beer radio, podcasts, video, events and more.